Original document(4 pages)  中文版
    This invention is by using of brown coal as a reducing agent for processing low iron content refined tin ore in the form of pellets, which are dried and reduced directly in refractories of reducing installations at reducing temp. of 850-1000 deg.C by maintaining for 2-3 hr. After the reduction is completed, the ground is separated mechanically or by stirring when moltening. After the separation, metal tin and a small amount of stannous silicate are obtained. With said process the whole processing is continuous, meanwhile, flexible in operation, slagless, saving of energy sources, lowering in first cost, no contamination, and economical profits are gained predominantly.
Application Number
申请号
85107123 Application Date
申请日
1985.09.21
Title 名称 To refine tin with brown coal
Publication Number
公开号
1009936 Publication Date
公开日
1987.04.01
Approval Pub. Date Granted Pub. Date
International Classification 分类号 C22B25/02
Applicant(s) Name
申请人
Yunnan Polytechnical College
Address 地址
Inventor(s) Name 发明人
Attorney & Agent 代理人 YANG HONGZHEN LIU TAIPING
More information 更  多  信  息


 Related patents information
Using lignite to smelt iron
lead-smelting Method without pollution problem
New energy-saving and nonpolluting process for antimony-smelting
Method for extracting tin from molten iron
Method for directly extracting metal Tin from low-grade Tin ore
Method and device for extract lead directly from galena
Method for direct extracting antimony oxide from low grade antimony sulphide ore
Method for making glass decorative wall hanging
Google
Note:All patent data come from State Intellectual Property Office of the People's Republic of China. If there were discrepancies between here and the State Intellectual Property office, the later is more accurate. The patent data is only for public exchange and learning purposes. We are not responsible for the adverse consequences with unverified use of the data.