    The present invention includes: smelting carbon semi-product in the steelmaking equipment; injecting that into the steel ladle; adding the slag-making materials, the reducing agent and the oxidation materials which contain alloy elements and are previously heat-treated into the steel ladle. At this time, the addition of the above-mentioned oxidation materials is started when the tapping amount of the carbon semi-products is not less than 0.25 of its total weight, but no less than 0.5, and the addition is carrying out during tapping of the above-mentioned semi-products and the addition is ended when the tapping of the carbon semi-products is completed. The reducing agent is added after the addition of the above-mentioned oxidation materials and the addition is finished before the tapping of the carbon semi-products is completed.
Application Number
申请号
88107940 Application Date
申请日
1988.11.18
Title 名称 Method of producing general-purpose steel
Publication Number
公开号
1042735 Publication Date
公开日
1990.06.06
Approval Pub. Date Granted Pub. Date
International Classification 分类号 C21C5/00,C21C7/04,C22C33/04
Applicant(s) Name
申请人
Donetsky Politekhnichesky Institut
Address 地址
Inventor(s) Name 发明人 Alexandr Georgievich Ponomarenko, Anatoly Yakovlevich Nakonechny
Attorney & Agent 代理人 XUE MINGZU
More information 更  多  信  息


 Related patents information
Google
Note:All patent data come from State Intellectual Property Office of the People's Republic of China. If there were discrepancies between here and the State Intellectual Property office, the later is more accurate. The patent data is only for public exchange and learning purposes. We are not responsible for the adverse consequences with unverified use of the data.