    In the process, soft coal is used as fuel and reducer with the ratio of lead sulfide mine powder: iron powder: soft coal=100:7-10:11-15. The process includes: grinding, mixing, smelting, slagging etc. with a smelting temp. of 1250-1350 deg.C, within a period of 7-9 hrs. The process is simple, equipment investment-saving, low energy consumption, suitable for commercial prodn., partic. for small-sized and medium-sized enterprises.
Application Number
申请号
89101983 Application Date
申请日
1989.03.30
Title 名称 Metal lead prodn. directly from lead sulfide mineral
Publication Number
公开号
1045995 Publication Date
公开日
1990.10.10
Approval Pub. Date Granted Pub. Date 1992.09.30
International Classification 分类号 C22B13/02
Applicant(s) Name
申请人
Zhu Songbo
Address 地址
Inventor(s) Name 发明人 Zhu Hai, Zhu Jianguo
Attorney & Agent 代理人 ZHAN XIHAN ZHU YUDAN
More information 更  多  信  息


 Related patents information
Google
Note:All patent data come from State Intellectual Property Office of the People's Republic of China. If there were discrepancies between here and the State Intellectual Property office, the later is more accurate. The patent data is only for public exchange and learning purposes. We are not responsible for the adverse consequences with unverified use of the data.