    The chemical preparation method for nickel-titanium alloy material, which is characterized in that: 1) covering the non-working position with soft nonmetal material to form protective layer; 2) dipping the alloy piece into reaction solution contained with hydrofluoric acid, nitric acid and water to required degree; 3) taking out and clearing the alloy piece in flowing water; 4) putting the piece in dehydrogenation furnace for one hour at 300Deg. This invention solves the rapid form problem failed by traditional technique.
Application Number
申请号
200410053734 Application Date
申请日
2004.08.13
Title 名称 Chemical process of nickel-titanium alloy material
Publication Number
公开号
1733974 Publication Date
公开日
2006.02.15
Approval Pub. Date Granted Pub. Date
International Classification 分类号 C23F1/04
Applicant(s) Name
申请人
Innovative Material and Devices, Inc.
Address 地址 200025
Inventor(s) Name 发明人
Attorney & Agent 代理人 zhao yongju

  
Environment protective additive used in metal pickling for delaying erosion, suppressing fog, and its manufacturing technique
Sheet metal having decorative pattern and method for manufacturing the same
Electroplating additive and its preparation method
Leveler compounds
Connecting terminal
Electricity conductive liquid capable of directly galvanizing the printed board
Japanese hop fiber for textile
Benne bioenzymatic degumming method
Extraction method of silk from silkworm silk gland
High-strength low-extension polyester staple fiber preparation method
Google
Note:All patent data come from State Intellectual Property Office of the People's Republic of China. If there were discrepancies between here and the State Intellectual Property office, the later is more accurate. The patent data is only for public exchange and learning purposes. We are not responsible for the adverse consequences with unverified use of the data.