The invention relates to a method for processing solid floor, which comprises: (1) drying wood that arranging the wood in drying furnace at 85-95Deg. C for 230-250hours; (2) molding that processing the dried wood into blocks; (3) secondary drying that drying the floor blocks into drying furnace to be dried at 85-95Deg. C for 7-9 hours; (4) immerging with paraffin boiling liquid that immerging the floor blocks in the paraffin liquid groove at 70-90Deg. C for 45-55 hours; (5) removing paraffin that arranging the immerged floor blocks on the support of drying furnace at 80-100Deg. C to remove paraffin for 7-9 hours; (6), furnishing that furnishing the block into final product. |