    The invention relates to hot-work die steel and its manufacturing method. It includes the following alloying element: 0.40-0.48wt% C, 0.60-1.00wt% Si, 0.30-0.80wt% Mn, less than 0.030wt% P, S, 2.20-2.70wt% Cr, 0.90-1.20wt% W, 0.80-1.00wt% Mo, 0.70-1.00wt% V, rest Fe and impurity. The method includes the following steps: adopting common steel facility, common medium steel smelting technology to smelt as the given constituent; forging; heat processing; making hot-work die. It has the advantages of reasonable alloy element composition, simplifying technology, lowering the cost. And it is fit for making tool die at 400-650 degree centigrade, such as cutting edge etc.
Application Number
申请号
200510118306 Application Date
申请日
2005.10.26
Title 名称 Hot work die steel and its preparation method
Publication Number
公开号
1912165 Publication Date
公开日
2007.02.14
Approval Pub. Date Granted Pub. Date
International Classification 分类号 C22C38/24;C22C33/04;B21J5/00;C21D1/18;C21D11/00
Applicant(s) Name
申请人
Maanshan Iron & Steel Co., Ltd.
Address 地址
Inventor(s) Name 发明人 Wan Weiguo;Peng Dacheng
Attorney & Agent 代理人 zhou zongru
More information 更  多  信  息


 Related patents information
Surfacing welding electrode for heat work mould
Composite shearing blade for shearing hot steel billet and its producing method
Steel for high strength shock-proof hot-rolled steel bar
Silicon-vanadium-nitrogen microalloyed medium carbon steel
Trace niobium -containing steel for cooling-control reinforced bar and method for producing same
Niobium titanium -combined microalloying steel for cooling-control reinforced bar and method for producing same
Google
Note:All patent data come from State Intellectual Property Office of the People's Republic of China. If there were discrepancies between here and the State Intellectual Property office, the later is more accurate. The patent data is only for public exchange and learning purposes. We are not responsible for the adverse consequences with unverified use of the data.