    The disclosed optical element comprises: a substrate with incidence and emergence surface, and a micro-pattern layer with lots of micro arc patterns combined with the emergence surface. The manufacture method comprises: preparing the substrate, coating resin, coining and forming, heating to form arc, and direct solidifying.
Application Number
申请号
200510098634 Application Date
申请日
2005.09.05
Title 名称 High molecular optical components with mini-pattern and method for manufacturing same
Publication Number
公开号
1928658 Publication Date
公开日
2007.03.14
Approval Pub. Date Granted Pub. Date
International Classification 分类号 G02F1/1335
Applicant(s) Name
申请人
Chi Lin Technology Co., Ltd.
Address 地址
Inventor(s) Name 发明人
Attorney & Agent 代理人 wanhua tang
More information 更  多  信  息


 Related patents information
Method and apparatus for extruding out and blow moulding
Nano polymer composite material and its prepn.
Method of removing As from water
Process for preparng simply dextrinized starch as powerful water absorbing and preserving agent
High molecule water preserving agent and its preparing method
Diffusion plate used in direct-type backlight module and method for making the same
Method for manufacturing high molecular optical components with mini-pattern
Dispersion brightening device
Compound dispersion device
Preparation method of cypressol metal compound
Google
Note:All patent data come from State Intellectual Property Office of the People's Republic of China. If there were discrepancies between here and the State Intellectual Property office, the later is more accurate. The patent data is only for public exchange and learning purposes. We are not responsible for the adverse consequences with unverified use of the data.