A preform (15) having a clad part of PVDF and a core part of PMMA is manufactured. The preform (15) is partially heated in a heating furnace (74) of 240 DEG C. The preform (15) is subject to the melt-drawing process to form a plastic optical fiber (17). The drawing tension to the preform (15) is measured by use of a drawing tension measure device (76). Based on the measured value, a drawing roller pair (78) adjusts the drawing tension to be 3.8 MPa. The plastic optical fiber (17) is fed via a dancer roller (82) and rollers (84, 86) toward a bobbin (87) to wind the plastic optical fiber (17). A winding tension measure device (85) measures the winding tension to the POF (17). Based on the measured value, the dancer roller (82) changes its position to adjust the winding tension to be 2.5 MPa. |
Application Number 申请号 |
200580010593 |
Application Date 申请日 |
2005.03.29 |
| Title 名称 |
Plastic optical fiber and method for manufacturing the same |
Publication Number 公开号 |
1938618 |
Publication Date 公开日 |
2007.03.28 |
| Approval Pub. Date |
|
Granted Pub. Date |
|
| International Classification 分类号 |
G02B6/00 |
Applicant(s) Name 申请人 |
Fuji Photo Film Co., Ltd. |
| Address 地址 |
|
| Inventor(s) Name 发明人 |
|
| Attorney & Agent 代理人 |
yuhui |
| More information 更 多 信 息 |
|
|
|